Dear Expert,


We have received A106 Gr. B seamless pipe with a visible seam. Refer attached photo. All the certificates and MTC' s are showing a seamless pipe.

We have done an etching test with the Nital solution, No visible weld fusion line is observed after the test.

Your expert advice Pls


--