Thursday, February 9, 2023

[MW:34010] SWPS FOR API GR46 AND X70

Dears, any one have SWPS for API 5L GR46 and X70 pipe please share me

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw_qOH_K5uCGwGmUy2VN%3DVDaawmpjOs-kU4K_of-zwCH5Q%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...