Hello Nikhil 

Both are P1 materials and can be welded together. 

Check QW-422 in sec 9.

On Friday, 20 January 2023 at 18:02:47 UTC+13 NIKHIL THOMAS JOY wrote:
Dear Experts,

Greetings of the day,

1. What is the Group number for S275JR? 

2. Already in steel structure WPS its mentioned applicable material A36,A53 Or Eq. WPS Mentioned Group 1 Only.
Is it possible to weld S275JR to ASTM A992 Gr.50?

I am requesting Experts' Technical input.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d3eca979-a2ca-484a-b272-5853b5cb479cn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...