Arc Welding is difficult, Brazing is possible. If fact a of copper to stainless joints are Arc Brazed with Silver Brazing filler . BAg 8 as cited by Mr Hegde  is a popular filler metal for such brazing. The most common option for joining  simpler shapes is Friction Welding , example as shown below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Cell/Whasapp:1-905-9793232

From: 'Prakash Hegde' via Materials & Welding <materials-welding@googlegroups.com>
Sent: August 25, 2022 9:19 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:33399] Re: Weld Copper to Stainless Steel 304

 

My opinion with experience Copper to SS welding is not compatible

You can braze or vaccine braze with BAg8 or similar  filler

Hegde

 

On Thu, 25 Aug 2022 at 18:04, 'J Prinsen' via Materials & Welding

You can try with inconel 625 or Nickel 200, or buttering the stainless steel with either 625 or 200 and then weld with the same consumable  to the copper

I' ve seen welding with a copper consumable in the past, but there is a high risk of hot cracks

 

 

Regards

 

Jurgen Prinsen IWE


Van: "Mohd Siraj" <mohd52100@gmail.com>
Aan: "materials-welding" <materials-welding@googlegroups.com>
Verzonden: Donderdag 11 augustus 2022 17:09:48
Onderwerp: [MW:33377] Re: Weld Copper to Stainless Steel 304

 

pl share exact specification of material to be weld with thickeness.

for any question to be answered quickly , you could provided suffiecent details so that other can understand your requirement like code interpretation querry.

On Saturday, July 30, 2022 at 5:00:55 PM UTC+3 Sohil Mehta wrote:

Dear Sir, 

Kindly suggest consumables for welding of Copper to Stainles Steel. 

Thank you.

 

Regards,

Sohil Mehta

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c84d8a39-6385-4d7d-9c48-df32d4658770n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2056395243.42875647.1661429976858.JavaMail.zimbra%40online.nl.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1295258517.2205182.1661433554582%40mail.yahoo.com.


 width=Virus-free.www.avg.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...