Re: [MW:33399] Weld Copper to Stainless Steel 304

Copper and Steel never formed solid solution. Try with Nickel buttering on both parts and then join with nickel 

Στις Σάβ, 30 Ιουλ 2022, 17:00 ο χρήστης Sohil Mehta <sohilmehta@gmail.com> έγραψε:
Dear Sir, 

Kindly suggest consumables for welding of Copper to Stainles Steel. 

Thank you.

Regards,
Sohil Mehta

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bf92e469-cb80-4285-bbfe-e23a4677e4b6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Dyf3ncLdnjkG02nxZmw-366959QcYm_Lp7AfyVt%3DEqzw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...