Thursday, August 4, 2022

Re: [MW:33363] Hardness - PQR Qualification - Acceptance Criteria for Weld Metal

Hi

Hardness acceptance based on client specification / NACE  applicable also for 
dissimilar metals 





On Thu, 4 Aug, 2022, 2:34 pm Sham Shahabuddin -Welding Inspector, HANBO, <shamshahabuddin.hanbo@gmail.com> wrote:
Dear Experts

Can anyone explain about the Acceptance criteria of Hardness for the weld metal. If my PQR is as per ASME SEC IX and if the hardness test is done, on what basis the test results are acceptable. 

Also please explain the same condition if we are qualifying dissimilar metals

Thanks and Regards 
SHAM SHAHABUDDIN
QC INSPECTOR - WELDING

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyAb6MBwCHpxM0OR-WJoddLhSvug8t6tP3fijAv5Dh-w482bQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzo-kuxOarnMLaF_br7zvWaGYT-o2c3c2jm_oCTc4miCrBbug%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...