[MW:33406] crack repair

Dears,

I have gate valve size 42" class 600 material WCB A216 and its manufacture according to MSS SP-55 casting and produce according to API 6D, i want to repair body crack so, can i know the procedure and standards that i must be dependent on for welding repair?