Wednesday, August 10, 2022

Re: [MW:33375] WELDER QUALIFICATION

Dear Mr. Saleem

Please note that as far the essential variables of the welder are within the ranges of the second WPS, the welder is qualified to weld using the second or any number of WPS.

Please note for welder qualification actual essential variable and the qualified essential variables alone are mandatory in the Report and the WPS used for welding coupon is non mandatory as per my knowledge.

Regards
Sham Shahabuddin 

On Wed, Aug 10, 2022, 6:39 AM manikandan J <mechmani22@gmail.com> wrote:
Dear All

   I have qualified welder in AWS D1.1, i have 2 WPS in aws d1.1 only changes the thickness limit but job thickness and process etc... is  acceptable limit the welder qualified, only changes is wps number. question is can i use the welder in second WPS as per AWS D1.1.

please give me a answer with reference from AWS D1.1

Regards,
saleem

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d1f5c1aa-55b8-4e02-a96c-d17466d12d48n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyAb6P-pDuGq%3D%2BSAUZmq4OKkb%3DN%3D3mU1eXcyL08mvDDDGjWmA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...