On Friday, 3 June, 2022 at 07:17:43 am GMT+4, Prasad rao <prasadrao31@gmail.com> wrote:


The above is applicable to both cap & root its clear in the above attachment 

On Wed, Jun 1, 2022 at 3:29 PM saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear sir


   Attached photo from api 1104. It's only for Weld caping visual? , there is any restrictions for root undercut in api 1104

Regards 
Saleem
--
Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmswphOU5QJXuzbV5-BexPkWd%3DAXbG%3DQr%3DqUjm5ri-bpfA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEML-XQi_HrTBwF8x33-AecxbgO5qZ%2BZeLZw7ousr2nT0W-Wpw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...