hi gents,
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb9b8ceb-4164-459d-ac06-9d51033706dan%40googlegroups.com.
can we do Magnetic particle test for duplex stainless steel
i believe we can do since DSS is ferromagnetic material
whats expert opinion?
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb9b8ceb-4164-459d-ac06-9d51033706dan%40googlegroups.com.
Comments