Dear Experts,

Please advise about the "Delivery conditions of the Plate" required to form a 2:1 Seli Ellipse Dish Heads with respect to the below specification.
1) Material Grade = SA 516 Gr.70
2) Minimum Required Thickness of the Dish Head = 70 mm
   Actual thickness suggest by the dish head supplier = 85 mm
3) Vessel Design Pressure = -28.88 to 121.11 Degree C
4) Service = Sour 
5) Dish head prepared by Hot forming with a tem.> 11°C of NR Tem. At Mill
6) Dish head will be Normalized @ 920 Degree C Max considered after forming.
7) Normalizing holding time shall be 1-1.5 Min/mm (Mill MTC / SPWHT)
8) Dish head prepared with a single longitudinal joint.

Thank You & Regards
Williams P Wilson
QA/QC Engineer
P Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ5xcx5%3Dg3PeqVt%2Ba1ZuWNX4Vw5gLeBHtJd%3DYoMuMcdutQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...