Re: [MW:33181] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Dear Raghuram,

Please any code case or Interpretation.

Thanks & Regards

J.Gerald Jayakumar




On Sunday, 26 June, 2022 at 07:46:29 am GMT+4, Raghuram Bathula <raghurambathula@gmail.com> wrote:


Although no restriction in code preferable methoud could custom build modular furnace (with panel construction) at site

It is straight forward method for cir seams, however for long seams you have to work a methodology for placing coils locally using WRC 452 guidelines, probably  supplimented with an FEA to check thermal stresses

On Sat, Jun 25, 2022, 8:21 PM <pgoswami@rogers.com> wrote:

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CADxVubnGTyb%2BFpEFzdoU3gq%2BBVcYGERP65xWkWxr7QM_Q6EmkQ%40mail.gmail.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...