Skip to main content

Re: [MW:33152] SA 387 GR 11 CL2 and SA 387 GR 22 CL2

Yes ,I too think the same way.
But want to understand /know what is followed  by other fabricaters when this condition arises.

On Fri, 17 Jun 2022, 08:49 'Prakash Hegde' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Hi
Its bit complicated
Does gr22 plates undergone simulation Heat treatment Generaly this Mail is QT and  Nr T is not prefered if NR T
 you require to carry NR T  and further PWHt on welded coupon and it is bit difficult to achieve property on weld by following NRT +pwht as per original plate Nr T (supplied condition
Generally such steel is welded using 9015EB3
Better go for crown and petal system for D end
What is the thk of Dend
Regards
Hegde

As 
You dont get Consumbles for 
a


les



On Thu, 16 Jun 2022 at 11:56, Vishwas Keskar Welding Manager  WELDING
Experts 

The dished end is to be fabricated with one number Chordal seam  for MOC of 
1) SA 387 GR 11 CL2
2)SA 387 GR 22  CL2

One  chordal seam in dished end is coming due  to plate  size( width) limitation  and the  diameter required of  dished end. So butt joint welding is to be done  followed by NDT .

Hot forming is planned . After forming is completed, separate   Normalizing and tempering Heat treatment is required as per Client specification.

PQR is to be established as per ASME SEC IX  .
Pl. suggest suitable consumable  and maintain strength 

Pl. share experience if any 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bd3a1f1c-6422-4640-985a-d05964ed96d5n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1840252717.3687373.1655390378527%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NJjR_m5Phssme0mZM4VbUzDj6QRYjW%2BRT5uY-Or8iDOg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...