Saturday, June 25, 2022

Re: [MW:33177] RE: PWHT Segment Wise for 9 Meter Dia Vessel

What diameter can your furnace accommodate?. 9 Meter seems to be Big.

There are some options if your Furnace cannot accommodate.

1.  Try for a Temporary furnace with proper insulation and Heating arrangements. Hope there are some subcontractors available.
2. Try for LOCAL PWHT of the seams.
3. Below option may be useful if you have difficulty accommodating the Length in one Heat.

Thanks & Regards

J.Gerald Jayakumar




On Saturday, 25 June, 2022 at 06:57:06 pm GMT+4, pgoswami@rogers.com <pgoswami@rogers.com> wrote:


Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAD9ib%2BzVU4dRb/ePF01LBnGAQAAAAA%3D%40rogers.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...