Re: [MW:33152] SA 387 GR 11 CL2 and SA 387 GR 22 CL2

Yes ,I too think the same way.
But want to understand /know what is followed  by other fabricaters when this condition arises.

On Fri, 17 Jun 2022, 08:49 'Prakash Hegde' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Hi
Its bit complicated
Does gr22 plates undergone simulation Heat treatment Generaly this Mail is QT and  Nr T is not prefered if NR T
 you require to carry NR T  and further PWHt on welded coupon and it is bit difficult to achieve property on weld by following NRT +pwht as per original plate Nr T (supplied condition
Generally such steel is welded using 9015EB3
Better go for crown and petal system for D end
What is the thk of Dend
Regards
Hegde

As 
You dont get Consumbles for 
a


les



On Thu, 16 Jun 2022 at 11:56, Vishwas Keskar Welding Manager  WELDING
Experts 

The dished end is to be fabricated with one number Chordal seam  for MOC of 
1) SA 387 GR 11 CL2
2)SA 387 GR 22  CL2

One  chordal seam in dished end is coming due  to plate  size( width) limitation  and the  diameter required of  dished end. So butt joint welding is to be done  followed by NDT .

Hot forming is planned . After forming is completed, separate   Normalizing and tempering Heat treatment is required as per Client specification.

PQR is to be established as per ASME SEC IX  .
Pl. suggest suitable consumable  and maintain strength 

Pl. share experience if any 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bd3a1f1c-6422-4640-985a-d05964ed96d5n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1840252717.3687373.1655390378527%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NJjR_m5Phssme0mZM4VbUzDj6QRYjW%2BRT5uY-Or8iDOg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...