Re: [MW:33148] SA 387 GR 11 CL2 and SA 387 GR 22 CL2

ER 90S B3

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Jun 16, 2022 at 11:56 AM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
Experts 

The dished end is to be fabricated with one number Chordal seam  for MOC of 
1) SA 387 GR 11 CL2
2)SA 387 GR 22  CL2

One  chordal seam in dished end is coming due  to plate  size( width) limitation  and the  diameter required of  dished end. So butt joint welding is to be done  followed by NDT .

Hot forming is planned . After forming is completed, separate   Normalizing and tempering Heat treatment is required as per Client specification.

PQR is to be established as per ASME SEC IX  .
Pl. suggest suitable consumable  and maintain strength 

Pl. share experience if any 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bd3a1f1c-6422-4640-985a-d05964ed96d5n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNFg1O7oZxYueY7mSL5xZHCoMKnzADoGfK%2BK%3Ddxo6gJSA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...