Re: [MW:33128] Re: FILLER AND ELECTRODE AS PER THIS MATERIAL

What is the base thickness

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Jun 13, 2022 at 8:53 AM Mohd Siraj <mohd52100@gmail.com> wrote:
yes this material quite common to qualify P1G1/G2 qualification in one go!..
you can use ER70S-3 and E7018-H4R...with preheat/pwht applicale as per asme-ix.

On Monday, June 6, 2022 at 6:31:44 AM UTC+3 sujit kumar wrote:
Dear all
Good morning.
I want to qualify PQR for  SA516 GR 70  which electrode and filler wire i should use for that Qualification..??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9fec5937-0720-42ef-823e-9e0a051ce9a2n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMQA3kfXbRwzrBvNVMeWw7DDc-p-%3DhvgvThFdwEk9ecAA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...