Dear Rao,
Thanks for the advise.

Can you please share as per which code we need to do a PQR coupon  and what mechanical/ NDT tests need to perform for qualifying WPS. 

On Sunday, June 26, 2022 at 9:23:47 AM UTC+3 srinivas rao wrote:

Dear Vinu,
Most commonly used welding process's for  rail welding is 
1. Flash butt welding process  
2. Thermit welding process 

Regards,
Srinivasarao
Welding engineer , GPS 
On Friday, June 24, 2022 at 2:31:50 PM UTC+4 vinu raveendran wrote:
Dear Experts,

Please advise what welding process is recommended to join rail material A75 (DIN 356) and as per which reference code/standard. Also mention what NDT to be performed.

--
VINU RAVEENDRAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8169d4ca-152f-4f16-8b73-6fe4a67e22e1n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...