Re: [MW:33013] Fwd: WPS TO QUALIFY THE OF THE WELDER

Hi,
As per Table QW451.4 All Groove weld test qualified for All fillet sizes on all base metal thicknesses and all diameters.


Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


On Friday, April 1, 2022, 10:11:08 AM GMT+7, Rene Alvarado <rene.alvarado.lozano@gmail.com> wrote:


FE DE ERRATAS

 

Can I use a WPS qualified with the SMAW process in position 6G on pipes Copper Nickel to Carbon Steel with a thickness of 0.237" and with backing ring to qualify the skill of the welder in fillet welding with the SMAW process in position 5F on pipes Copper Nickel ( O.D. 2 ½" thickness 0.280") to Carbon Steel (O.D. 3" schedule 160 in accordance ASME IX?

 

Thanks

---------- Forwarded message ---------
De: Rene Alvarado <rene.alvarado.lozano@gmail.com>
Date: jue, 31 mar 2022 a la(s) 08:40
Subject: WPS TO QUALIFY THE OF THE WELDER
To: <materials-welding@googlegroups.com>


Experts

 

Can I use a WPS qualified with the SMAW process in position 6G on pipes Copper Nickel to Carbon Steel with a thickness of 0.237" and with backing ring to qualify the skill of the welder in fillet welding with the SMAW process in position 6G on pipes Copper Nickel to Carbon Steel with a thickness of 0.125"  ?

 

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAHbC_j1M2mbAJbiCsAfyikj-CPst%2BEtPqr%3Dm9nA6Oh5Hg_tQkA%40mail.gmail.com
.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...