Re: [MW:33054] P11 material hardness value

Inline image

Please give some details regarding below, as anyone in the Group may provide solution to you.

1. Hardness Location (Weld & HAZ)
2. Type of Hardness Test, Vicker's, Brinell or Rebound Hardness Tester.
3. PWHT cycle, soaking temperature, Time, Heating Rate & Cooling Rate.
4. Welding Heat Input
5. Maximum temperature in The Tubes(steam)
6. Any additional details which you may feel may be useful.

380HB is way out of Rectification and let's seek experts advise.

Thanks & Regards

J.Gerald Jayakumar



On Monday, 25 April, 2022, 11:49:16 am GMT+4, Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:


Dear james,

Good morning, 

Please find the below details, the following issue is related to the boiler steam drum tubes

  Base Tube material: A213 T11

  Obtained hardness value after PWHT : 380HB

  WPS value: 238HB
  
Thanks & regards
Chiranjeevi Anil


On Mon, 25 Apr 2022, 05:47 'james gerald' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Pls provide some additional details.
Hardness values obtained.
Base Pipe/ PQR / Production Hardness

Thanks & Regards

J.Gerald Jayakumar




On Monday, 25 April, 2022, 07:13:14 am GMT+4, Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:


Dear experts,

We have an issue in the hardness value for P11 material of pipe.

If the value exceeds what are the matigations required.

Kindly advice

Thanks and Regards
chiranjeevi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0y-8DmngFND-R1R%3D%2BYCoCDJURQwGOeA5Cb2M8HJAouxrw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2070032876.517367.1650861559056%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zpeD86MdwUM9Qy7%3DMds5tEKNjbP2tOey%2BvHZ0GUyy0wA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .