Dear,
U can use ERCuAl-A2 
Take care if the pump working in heavy corrosive fluid , then impeller to be heat treated after welding repair


Best Regards ,
ENG. Ahmed Osman



On Tuesday, November 16, 2021, 06:33:25 a.m. GMT+3, alexcalangi.cpmcgsi@gmail.com <alexcalangi.cpmcgsi@gmail.com> wrote:


Dear Experts,

 

We have a pump impeller with crack for repair. The material specification for this impeller is Aluminum Bronze Casting (AlBC3 / ASTM C95800).

 

With this regards, what should be the appropriate welding filler or electrode to be used for this type of material?

 

Thanks in advance for your support.

 

Best regards,

Alex

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/001f01d7da9a%2478e3e920%246aabbb60%24%40gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...