Re: [MW:32603] Pickling and Passivation of Hastelloy

Yes it is mandatory to resist these we have to restist % of oxygen during welding .
Reason is this there is a chances of formation of oxide on weld and adjascent area heat sinks marks found with defferent colour which highlights a depletion of corrosive property.
By pickling passivation its help to reform that llayer and safe material and weld.
Its shouod be general practise no need to mention it as a stage in itp.
As per our manufacturing practise we did it regular basis and got good results.
It will help after installation during service also.
Go for it frelly it helps.
I m sharing my experience not bookish lines

On Thu, 11 Nov 2021, 7:11 am Maulik Thakkar, <mlkthakkar2@gmail.com> wrote:
Dear all,

Can any one suggest picking and Passivation procedure for Hastelloy?

After Heat Treatment and After Welding.

Is it mandatory to perform Picking and Passivation?


Please provide literature or Standard if any.

Regards,
Maulik

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFK0MUN6exyioEi6hTNsP%2BbQ%2BFecVSsCUSWx0Sk-qY_pgqsatQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k8PX4RoMvnzq6UQ%3DC%2BoKbBt0%2BfBZXVQaQzs2seAFTG37w%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...