[MW:32590] PQR TEST FAILURE

Dear masters 
durring the mechanical tests for our WPS 
1- piping B31.3 
SS to DSS  TEST COUPON 2" thk 3.05 mm 
EE.PNG

in the bending test with 4 test one is failure rejected  
so in this case IS IT ACCEPTABLE 

ALSO FOR ANOTHER PQR  
2- PIPING B31.3 
CS TO CS PIPE TO FLANGE  API 5L GR B TO ASTM A105 
PMOM.jpg
THE FAILURE IN HAZ OF FLANGE  WHAT IS THE ACCEPTABLE HERE

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ce990b20-a027-482c-9d55-2d6023725422n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...