Saturday, November 6, 2021

[MW:32591] WPS for SA387 Gr F11 CL2

Dear All,

Can someone give me WPS for SA387 Gr F11 CL2
Thickness : Shell 30mm & dished end 35mm
PWHT required as per code.
3mm SS.304 cladding from inside.

Regards,

Uday

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2e49c943-fa00-414c-ab11-84bf251115bfn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...