[MW:32591] Alternative MOC - SA387 + SS.304 cladding to complete SS.304

Dear Experts,

Vessel MOC = SA387 GR F11 CL2 + 3mm SS.304 clading
Max operating Temp = 425 C
Max Pr = 20 bar (g)

Can we replace above moc with SS.304.
Will there be Sensitization issues a this temp ??