Re: [MW:32607] Digest for materials-welding@googlegroups.com - 1 update in 1 topic



On Tue, Nov 16, 2021 at 10:22 AM <materials-welding@googlegroups.com> wrote:

           Dear Mr Alex
 Your material 95800 is commonly used Al Bronze with Nickel .  It is used for sea water service.

 Please use matching grade electrode /wire conforming to AWS ECuAlNi/ERCuAlNi grades
A well known brand to suit is  AMPCOTRODE 46  electrode and AMPCOTRODE 46 wire.
You can use any other brand too as long it is as per AWS standard.



<alexcalangi.cpmcgsi@gmail.com>: Nov 16 11:31AM +0800

Dear Experts,
 

 
We have a pump impeller with crack for repair. The material specification
for this impeller is Aluminum Bronze Casting (AlBC3 / ASTM C95800).
 

 
With this regards, what should be the appropriate welding filler or
electrode to be used for this type of material?
 

 
Thanks in advance for your support.
 

 
Best regards,
 
Alex
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMrhEo_Sz6JZdhmLr9pTXN_XnQPHjJQmF%2B1Wb9bWoF_nxa5VAA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...