[MW:32606] Pump Impeller crack repair

Dear Experts,

 

We have a pump impeller with crack for repair. The material specification for this impeller is Aluminum Bronze Casting (AlBC3 / ASTM C95800).

 

With this regards, what should be the appropriate welding filler or electrode to be used for this type of material?

 

Thanks in advance for your support.

 

Best regards,

Alex