How much flared dia from to which dia 
What is % ?

On Thu, 11 Nov 2021, 08:41 Raja Pandiyan, <krajapandiyan@gmail.com> wrote:
Dear experts,
Pl clarify the heat treatment requirements for SA106 Gr.B pipe I.D  to be flared and done by hot formed operation  like red hot heating with hammering of die in the pipe id  to get the required dimensions.

Does it require heat treatment?

Also the above said process is good engineering  practice for flaring operation of pipe? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADuMvPb%3DddCgS030uK6pZaqS5KnVyeHMG41Vp-rZo29%3DzRAT4w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3POvW2Jf2Dwbdq5aM3Wp8s3djopP0X_YP1PyL-TTzvMYw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...