   Bend and impact test failure means that you have more interpass temp during welding. And also undercuts between passes and not cleaning between passes.
 
We can infer the following:
1. Welder and inspector did not pay attention to interpass temp in an attempt to complete the joint faster. 
2. Welder welded with high voltage arc which created undercuts on the weld joint face and did not remove those undercuts by grinding.
3. Heat input during welding was not calculated and maintained during welding.
4. Check the compatibility of filler metal used for welding this dissimilar joint. 

The only way is to re weld another pqr with following corrections. 


Regards,

Charles. 

On Fri, Nov 5, 2021, 5:53 PM QA/QC <adnanziad49@gmail.com> wrote:
Dear masters 
durring the mechanical tests for our WPS 
1- piping B31.3 
SS to DSS  TEST COUPON 2" thk 3.05 mm 
EE.PNG

in the bending test with 4 test one is failure rejected  
so in this case IS IT ACCEPTABLE 

ALSO FOR ANOTHER PQR  
2- PIPING B31.3 
CS TO CS PIPE TO FLANGE  API 5L GR B TO ASTM A105 
PMOM.jpg
THE FAILURE IN HAZ OF FLANGE  WHAT IS THE ACCEPTABLE HERE

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ce990b20-a027-482c-9d55-2d6023725422n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKpzM4BsyYoGO%2B9q5k8raoBEDd6Y1WHoTZhAEKJAd3UN6%2BYW6w%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...