Sunday, October 31, 2021

Re: [MW:32589] SA 516 GR 70- AVOIDANCE OF PWHT - 40 mm thickness

Refer attached interpretations

On Sun, 31 Oct 2021, 10:30 Vishwas Keskar, <vvkeskar123@gmail.com> wrote:
Thanks for Sir.
Pl help for ref for Code or Code case.

On Fri, 29 Oct 2021, 21:40 pgoswami, <pgoswami@rogers.com> wrote:
Sec VIII,Div1:-
40 mm thickness calls for PWHT irrespective of service,  lethal or Non- Lethal. 
Would like to see in  DIV1,which code clause or code case,  allows application of buttering on C.S, PWHT of individual sections, welding of the closing seam by austenitic filler metal with no PWHT.

Thanks. 
P.Goswami. 




Sent from my Bell Samsung device over Canada's largest network.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/617c1ce1.1c69fb81.e31de.34e7SMTPIN_ADDED_MISSING%40gmr-mx.google.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3N4t9gCO%2B_BeK9hm%2Bh8G-U1tcHrxSHzqOyrmLiOqwxLFA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3ZiHHg2VaOd_y6wKpiMpV3aY%3DoutaZPH2DB6rhQ2zB0%2BQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...