Re: [MW:32588] SA 516 GR 70- AVOIDANCE OF PWHT - 40 mm thickness

Dear Prasad 
Thanks for technical support.
Pl share where this was deployed.
Our vessel is ASME SEX VIII DIV 1 vessel
U stamping and TPI is involved.
Any Code back up , Code case  will be further helpful .

On Sun, 31 Oct 2021, 10:30 Prasad Ghanekar, <prsgne@gmail.com> wrote:
Sir,
1. In this case buttering is carried out prior to PWHT
2. PWHT is due to thickness of P1 material
3. No welding involved with P1 material in closing joint
4. PWHT is not mandatory for P8 welds.

That's my analysis and understanding.
We have implemented such practice in past due to some construction constraints.

Regards,
Prasad G.


On Fri, 29 Oct 2021, 21:40 pgoswami, <pgoswami@rogers.com> wrote:
Sec VIII,Div1:-
40 mm thickness calls for PWHT irrespective of service,  lethal or Non- Lethal. 
Would like to see in  DIV1,which code clause or code case,  allows application of buttering on C.S, PWHT of individual sections, welding of the closing seam by austenitic filler metal with no PWHT.

Thanks. 
P.Goswami. 




Sent from my Bell Samsung device over Canada's largest network.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/617c1ce1.1c69fb81.e31de.34e7SMTPIN_ADDED_MISSING%40gmr-mx.google.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3b9ENgcV8DhsRJg2S%2B82%2B3FsVtHRndeQbV5VxunJKcNRw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3P_JS_krsoJuCXtY9fG%2B-G3nAQKQih0MU3wrX6NiZCSCw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...