Monday, October 25, 2021

Re: [MW:32575] Cladding UNS 32750 verification of consumable used

Send tabular excel sheet with material MOCs and type of joint .
Address service conditions such as 
temperature ,corrosion atmosphere ,

regards 

On Mon, 25 Oct 2021, 08:44 Muhammad Azeem, <azeem7999@gmail.com> wrote:
Dear Experts ,
I need your kind advise on priority basis as per below mentioned query raised by our vendor ..


We have considered the following filler wire for girth welding of various
combination. Pl confirm the same.
For serial number A & B : ERNiCrMo‐3 (UNS N06625)
For serial number C : ER 2553 (UNS 39553).
A. Carbon Steel (P1 Gr 2) with UNS S32750 CRA Overlay to UNS S32750(D.S.S)
Solid Alloy Branch connection
B. Carbon Steel (P1 Gr 2) with UNS S32750 CRA Overlay to Carbon Steel (P1 Gr 2)
with UNS S32750 CRA Overlay.
C. UNS S32750 (D.S.S) Solid Alloy Girth welded Joints.


My Suggestion 
the suitable filler wire.
ERNiCrMo‐3 (UNS N06625) / ERNiCrMo‐8 (UNS N06975) is
acceptable to weld for serial
number A & B. with reference to
corrosion 

ER 2553 (UNS 39553)  / ER 309LMO  is
acceptable to use for serial
number C
if only PREN value of
weldment is more than 42

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/439c3117-485d-45fa-a059-2ae8dd018466n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3O3DnvSQGM9biQAcGZ5dsX-oqXpVbpwK6-K7XVqJdP_zA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...