Re: [MW:32561] ASME B31.3 process piping Hydro in Lieu of RT

tie in must to be radiofraphie or other NDE and its not include in hydro test 
As per Para 345.2.3 (c) of ASME B31.3 you can either do 
100% RT or 100% UT. If Project Specification asks for, you may have to 

On Thu, 14 Oct 2021 at 14:25 Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:
Dear Experts ,
due to time concentrate we are unable to do the RT as we need to arrange the RT crew and ID's process for site access  ...........

as per drawing 5% RT is required .

we can perform hydro of tie in joints ? 

can you please advise for the reference from ASME B31.3  ? 



Best Regards,
Zafar Iqbal 
00966544639978 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XcM6-QrnGrGm5%3DBN46HRJx_k6DKiaPBs6Pbpjw033JPSA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACbfGKeF7kMKtvFc8Zq33KX69xUcLNwJO_9sAfydzyCct4nfjQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...