Friday, October 15, 2021

Re: [MW:32561] ASME B31.3 process piping Hydro in Lieu of RT

Hi, 
There's one option in B31.3,- U341.4.1.
A weld coupon examination in accordance with para. U344.8 May be used in lieu of 5% random radiography/ultrasonic examination required in para. 341.4.1(b)(1) when the following  are employed in fabrication.
1. Autogenous automatic welding 
2. Automatic orbital welding with the use of consumable insert rings.

There is no option for hydrostatic in lieu of RT.

Karthik


Sent from Yahoo Mail for iPhone

On Friday, October 15, 2021, 1:13 PM, Karthik <karthik6684@yahoo.com> wrote:

Hi, 
There's one option in B31.3,- U241.4.1.
A weld coupon examination in accordance with para. U344.8 May be used in lieu of 5% random radiography/ultrasonic examination required in para. 341.4.1(b)(1) when the following  are employed in fabrication.
1. Autogenous automatic welding 
2. Automatic orbital welding with the use of consumable insert rings.

There is no option for hydrostatic in lieu of RT.

Karthik


Sent from Yahoo Mail for iPhone

On Thursday, October 14, 2021, 8:25 PM, Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:

Dear Experts ,
due to time concentrate we are unable to do the RT as we need to arrange the RT crew and ID's process for site access  ...........

as per drawing 5% RT is required .

we can perform hydro of tie in joints ? 

can you please advise for the reference from ASME B31.3  ? 



Best Regards,
Zafar Iqbal 
00966544639978 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XcM6-QrnGrGm5%3DBN46HRJx_k6DKiaPBs6Pbpjw033JPSA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...