Re: [MW:32550] IMPACT TEST FAILLURE

No it is not,

Something went wrong with the thermal cycle during welding, heat-input/interpass to high will break down the impact thoughness

Regards


Jurgen Prinsen IWE
Metallurgist and welding engineer



Van: "QA/QC" <adnanziad49@gmail.com>
Aan: "materials-welding" <materials-welding@googlegroups.com>
Verzonden: Donderdag 7 oktober 2021 10:16:23
Onderwerp: [MW:32549] IMPACT TEST FAILLURE

DEAR MASTER 
we have a test coupon 7.11 thichness with flange a106 with a105n 

during mechanical test the impact test for FLANGE FAILLURE IN HAZ  IN 3 POINT £

IS IT ACCEPTABLE 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b6717387-54eb-4c06-9748-9d4eddf4497dn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...