Re: [MW:32545] Acceptance criteria for distortion

The distortion may be due  to lack of sufficient Stiffeners and supports.

Normally the Type of Distortion which occurs is as below.


Inline image



There are no specific requirements to Distortion while qualifying the WQT. Even WQT's of pipes are being successfully Radiographed. Hence as long as you are able to Radiograph 6inch (150mm) successfully, WQT is considered acceptable.

Thanks & Regards

J.Gerald Jayakumar




On Friday, 1 October, 2021, 02:06:33 pm IST, Samiulla Syed <ssyed@niti.edu.sa> wrote:


Dear Expert

Can some help to get the distortion acceptance criteria to WQT at 4G position.

--

--
Best Regards
Samiulla Syed,
Senior Trainer,
Welding Department,
TUV Rheinland Arabia LLC
National Industrial Training Institute,
Al Ahsa,
Eastern Province,
Kingdom of Saudi Arabia,
Email: ssyed@niti.edu.sa
          qcsyedsami@gmail.com
Mobile: +966(0)595531593.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFRNJK8xjqNeVZqH8mPSiJXiGOeyRarkk%3Dj3qytygKrBKVVRMA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...