Wednesday, October 27, 2021

[MW:32576] Heat Treatment of 25CRMo4

Dear Sir
Can you provide me with the actual holding time for heat treatment of rod with diameter of 170mm  as the material is 25CrMo4  
i need to apply hardening at 840C but i don't know the appropriate holding time matching with the diameter of 170mm
Thanks in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fae61d6b-5a88-405d-b9ce-5c68c00e4356n%40googlegroups.com.