Re: [MW:31991] ASME B31.3_2018- Table 331.1.1-PHWT minimumn Holding Time for base material thk-75mm

2 hours for 50 mm additional 15 minutes for 15~20 mm.

On Fri, Feb 5, 2021, 1:33 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
based on toughness requirement

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Feb 5, 2021 at 8:36 AM Chandru Sekar <chandruyou25@gmail.com> wrote:
Why they segregated as group and in which basis ?

On Thu, 4 Feb 2021, 08:31 Anban, <gane2478@hotmail.sg> wrote:
Dear Experts

Need your guidance in understanding  PWHT minimum  Holding Time base material thk.-65 ~ 75mm

P-No. 1, Group Nos. 1–3
Minimum Holding Time at Temperature for Control Thickness [Note (2)]
-Up to 50 mm (2 in.)-1 h/25 mm (1 hr/in.);15 min min.
-Over 50 mm (2 in.)-2 hr plus 15 min for each additional 25 mm (in.)


Best Regards
Ganesan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b538da9f-4e78-4b7c-85c3-7679328ed9bdn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGWOcnqMNXcWFH-bUvTt7GM1yoJJC6o5fUR_aKy3aWTuQs5fPQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePRn47pM%3DPoLYZDZnLE7eZPXYuDS%2B-AcVjtQnM44uotJQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BHpzU7wxr%2BY4hNcuFtXEGmBFL5dfJwRhNhheU1%2Bfxsaf4K9Hw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...