Wednesday, February 3, 2021

Re: [MW:31976] Accuracy of PMI

Tolerance allowed 

On Tue, Feb 2, 2021 at 7:47 PM Pravin Poornachandran <htcispravin@gmail.com> wrote:
Dear expert, 

Good day. 

Recently I performed WPS for ER70S-G for nace requirement project. 
Based on welding consumable mill certificate as per EN10204 3.1, Ni <1% and these chemical analysis is conducted in authorised laboratory following the method specified in industrial code. It is laborious procedure and accurate. 

But when we perform PMI, Ni values shows 1.2-1.5, which client is questioning now. 
I did contacted consumable supplier and they are very certain Ni is less than 1%. 

Can anyone advice how should I handle this situation. 

Best regards,
Pravin Poornachandran 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7cJnBBffbUGsDUJKPoFzVRvnQ-yOkMV89Ur_sGJiPcemQ%40mail.gmail.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUM%3DXXg2dC3v3o%2BO7Mc85zhZXdMdGrjki85iSdCqgpetyg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...