Sunday, February 14, 2021

[MW:31992] Welding between api 5l X60 to AISI 4130

Dear All,
Refer to below mail there is small correction * low alloy steel 


On Sun, 14 Feb 2021 at 10:31, seejo nereparambil
<seejonj@yahoo.com> wrote:
Dear Experts,
We are in process of Proceedure qualification for CS to Low carbon steel. Hence ,i am seeking your advise to select suitable welding electrodes for  welding between AISI 4130 to API 5L X60 material
Design code is ASME B 31.3 and qualification in accordance with SecIX, thickness is 14.27 mm

Kindly provide your recommendation 

Rregards
Seejo



On Thu, 4 Feb 2021 at 11:38, sunil kaushik
<sunilkaushik08@gmail.com> wrote:
PMI is the sorting method .you shoul go for the wet analysis testing.

On Wed, 3 Feb, 2021, 9:17 am Pravin Poornachandran, <htcispravin@gmail.com> wrote:
Dear expert, 

Good day. 

Recently I performed WPS for ER70S-G for nace requirement project. 
Based on welding consumable mill certificate as per EN10204 3.1, Ni <1% and these chemical analysis is conducted in authorised laboratory following the method specified in industrial code. It is laborious procedure and accurate. 

But when we perform PMI, Ni values shows 1.2-1.5, which client is questioning now. 
I did contacted consumable supplier and they are very certain Ni is less than 1%. 

Can anyone advice how should I handle this situation. 

Best regards,
Pravin Poornachandran 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7cJnBBffbUGsDUJKPoFzVRvnQ-yOkMV89Ur_sGJiPcemQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA-uzKWwCk1yNyUfbMRbMO8AJfdd8pce4XdnxfpetqJiLgHvTw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/833242771.1076565.1613288159630%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...