Monday, February 1, 2021

[MW:31969] NACE SP0472-PWHT - AMINE service

Experts

Client Requirement : Vessel shall be PWHT. Production Weld deposits hardness shall not exceed 200HBW after PWHT. Carbon steel welds shall comply with NACE STD SP0472 para. 2.2 & 3.3

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a024d874-aeff-4042-afd5-cf7b8a6e2a62n%40googlegroups.com.