On Thu, Jan 21, 2021, 3:24 PM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
Construction Codes ( ASME SEC VIII DIV I , ASME SEC I )are silent about simulation PWHT.
Client specifications( like Aramco, PDO , Shell DEPs) are specifying these simulation PWHT requirements.
We have to anticipate possible   repairs after PWHT .
Accordingly PQR shall be established .


On Thu, Jan 21, 2021 at 12:23 PM sajeed zaheer <sajeed7674@gmail.com> wrote:
Hello Everyone,

As per Sec 8 code there is no were written about the simulation PWHT, but in the ARAMCO specification I'm  encountering  with  this simulation PWHT,  Two PWHT cycle to account for future repair.Please clarify my doubt about the simulation PWHT.

Virus-free. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFycdMz3UY6_LM9Ot8f%3Dj2NBSKU%2B1XnNgmVeWLAhcZDupZVhhw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OSkBN2F02EaDj7FHs8JaHV-vuHxcySsHxhwU8bhgqzbw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP%2BeN2ktaWxynjmQxXTOxyswrHydhy_tW-qkA4gn-DJtA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...