Sunday, January 17, 2021

Re: [MW:31934] RE: 24729] Welding of SB729 UNS NO8020


ER320LR is matching consumable . Weld with due care .
 ERNiCrMo-3  is aslo acceptable
On Saturday, April 23, 2016 at 8:28:07 AM UTC+4 kannayeram gnanapandithan wrote:
no, u may use 317 which is readily available in the market

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Sat, Apr 23, 2016 at 12:40 AM, rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA <rajesh....@gmail.com> wrote:
Dear sir,
     Thank you very much for your reply.ER320 LR is not available in our area so can i use ERNiCr-3 for welding of alloy 20 ?
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/652200f9-45d4-4150-86e3-110287051702n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...