These are straight Cr Stainless steels for high temperature application.
In boiler , you can use this material.
Pl. send what attachment part you are looking for ?


On Monday, January 25, 2021 at 7:42:58 AM UTC+4 Emad wrote:
Dear all,

what will happen to the grains of a ferritic stainless-steel type AISI 405 used as an attachment of a hanger bar in a boiler, when it is exposed to flame temperatures of the boiler for 4 years of continuous operation? It is understood that the 405 steel will not oxidize in the high-temperature service environment.

Regards,

Emad


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f2ee4edc-671c-4f44-82e8-092cf1fb1198n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...