Skip to main content

Re: [MW:31923] SS-316L Rusting

After degreasing any surface treatment required, otherwise after  approx 24 hours rusting of material starting,

On Sat, Jan 9, 2021 at 1:29 PM Adnan B.BELGACEM <adnanbb.psi@gmail.com> wrote:
Dear Jamie;

Yes, the passive treatment meets the requirement of the ASTM and vendor instruction for application steps, we need to know the main reason for these faults could be due to the below reason which under investigation:

1- Vendor product used is expired (Under verification with supplier)
2- Water used was contaminated (checked and found acceptable)
3- Environment condition such as sunlight (maybe is not the main reason)
4- Other
So for this case, we need to repeat the passive application or we should follow another applicable procedure to remove this rust and to avoid the recurrence. 

regards
Adnan

Le jeu. 7 janv. 2021 à 04:49, Jamie Reyes <jamiejrmachineco@gmail.com> a écrit :
Did this material/fabrication receive chemical treatments such as, but not limited to, pickle and passivate treatment? If so, do you know what test method was used to prove conformance to specification? Do you have the inspection report from the pickling and passivation, if performed? Depending where you are located, ASTM A967 is an industry standard specification for such treatments that shall be followed, or its equivalence.   

On Wed, Jan 6, 2021 at 7:24 PM Adnan B.BELGACEM <adnanbb.psi@gmail.com> wrote:
Dear Expert,
Please could you advise about the root causes and how we can repair and stop this rust that occurred after the degreasing of the SS 304L tank? 

Regards
ABB


Le jeu. 28 mai 2020 à 13:30, sachit yadav <sachit.baroda@gmail.com> a écrit :
Appears to be fluid marks due to contamination or possibly poor pickling done.

On Thu, 28 May 2020, 10:46 Vinod Kataria, <vinod.kataria@blissanand.com> wrote:

Dear Expert,

We have received an email from our customer with pictures showing "rust" on the stainless steel (SS-316L) chambers.  Can anyone please tell me what you see in these pictures from your perspective?

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/TY2PR0101MB29421148FFC32992DCB565C5878E0%40TY2PR0101MB2942.apcprd01.prod.exchangelabs.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAT7JJiAe6oS4_WGLSW9_iN5bF6K2jOgVf6agTWSGipZ_e2DNw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB68E5kHmYUDcySpQUz_PenstNbX6BH8aBxUMJUWLc%2BwPiQmBA%40mail.gmail.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUP%3DLwt-FoAouHWeJjSW%2BsFKXLQLR3JK%2BOuwZwRfN3guMA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB68E5kTUgZkfn%3DXVrcvnhSOne0%2B62-%2BGKdb2mwMR4-pEjJBvw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB7xyL2eE3tnch9AXr2T5whV68JE%2BvhC8GYEYK%2B0wdNwOkX-Kw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...