Dear Jamie,

WPS/PQR/WPQ was qualified in accordance with AWS D1.1

Yes the testing was done at an accredited third party lab and we have the test certificates from the lab stating that the PQR was used to qualify the welders.

On Mon, Jan 18, 2021 at 4:36 PM Jamie Reyes <jamiejrmachineco@gmail.com> wrote:
What was the code that was used to qualify the WPS/PQR/WPQ?

Were the PQR/WPQ test specimens tested at an accredited third-party lab? If so, do you still have the test certifications from the third-party lab stating acceptance, with the PQR that was used and other info etc. noted on the test certification(s)? 







On Sun, Jan 17, 2021 at 7:05 PM 'Anumiah Veera Jegan' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Dear all,

We currently have a WPS with us.But due to some documentation error the PQR was lost.Is the WPS still valid(we've been using it for years).Does this also make the welders qualified based on this WPS invalid?.Thanks

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d5e7f7ec-afee-4dc8-8581-58a09910c26cn%40googlegroups.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUP75NgtpZXZetbdvkv_Vqgt4wK%2B1eqdMdafGV3vTrc3uw%40mail.gmail.com.


--
Displaying
Regards,
Anumiah Veera Jegan
Certified Welding Inspector
Ley Choon Group
No 3 Sungei Kadut Drive Singapore 729556
Office Tel: (65) 6757-0900 | Fax: (65) 6757-0100
Website: www.leychoon.com

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEQjo%2BS5QNutDm02CetgGh_78V%2BnJ9UwH7SDi27MFho%3DaV6Mmg%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...