Thursday, January 21, 2021

Re: [MW:31945] Overcoming distortion in SS 304L pressure vessel

Hi
You can also use water jet opposite side during welding to control distortion in SS304 L and proper stiffening due to lesser thickness.

Regards
Ajay Gupta




On Thu, Jan 21, 2021 at 8:43 AM Shahil Saini <sainishahil98@gmail.com> wrote:
Hello everyone, 

How to overcome the distortion in pressure vessel of material SS 304L?, having thickness 8mm of two dish-end and shell having thickness of 6 mm, I am attaching photographs of vessel for your reference,



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_931zTtSjSuhEit%3Dc-5afiAF3nAzqXgUU%3DK53y2oG6A_Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMBBuP1M9cLq4X39NuGaV5YSTBdVKLwOESrUUbES6ntDYf3Y8Q%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...