Tuesday, January 5, 2021

[MW:31914] Welding of Trunnions Brackets Assembly Q355C & 42CrMo

Dear Experts 

 

we had design one Bracket assembly for holding one Hammer trunnion 

 

the Pin is grade 42CrMo H+T (EN 19) and bracket plates are grade Q355C (S355) 

 

Project is asking for WPS/PQR for these 2 materials welding together? and we have only WPS/PQRs for S355 and API X52 

 

You feedback with references will be highly appreciated

 

Regards,

HA 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzctgaab%2BzJbxcnxpYO6kGr1QShAdhsdhdAu%2BK9HqFRseQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...