You cannot carry out destructive testing on the job weld after heat treatment to assess effect of heat treatment on mechanical properties.
Hence test coupons are welded exactly following the same welding cycle/ process as that of job weld and along with job.
These teat coupons undergo heat treatment along with job weld. Destructive testing is carried out on the test coupons to assess the effect of heat treatment on the weld. If mechanical properties are meeting specified requirements, the joint is OK. If not reweld the joint & carry out heat treatment again,carry out destructive testing.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...