This is special welding technique. TB technique is used mainly for weld repair on C.S& LAS ,in avoidance of PWHT. Hence correct metallurgical evaluation of the material to be repaired  is a must before proceeding.

 

NBIC code provides detailed guidelines on how to develop an procedure. Sec-IX QW-290 provides guidelines on how to qualify a procedure.

 

Following article describes many pros and cons about this method and may help you to get a feel of this technique and move forward.

 

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Saudi Aramco: Designated Project Welding Engineer(DPWR)& Quality Management Personnel

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

http://www.weldfabtechtimes.com/article/__trashed-2/

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of joydev dalai
Sent: January 17, 2019 10:33 AM
To: materials-welding <materials-welding@googlegroups.com>
Subject: [MW:28925] Welding procedure for Temper Bead Welding method ( QW 290)

 

Dear All,

 

Please share me Temper Bead Welding method.

 

--

 

 

Best Regards,


Joydev Dalai

Dy. Manager - QA/QC

+91-6202987794

Kalpataru Power Transmission ltd.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...